Quantitative assessment of the oxidation potential of sulfide-bearing aggregates in concrete using an oxygen consumption test
详细信息    查看全文
文摘
In the presence of oxygen and humidity, the iron sulfide minerals present in some concrete aggregates can oxidize creating damage to concrete infrastructure. An oxygen consumption test was developed to assess the oxidation potential of concrete aggregate. A compacted layer of aggregate material is exposed to oxygen (O2) in a hermetic cell, and the O2 consumption is monitored. Optimized parameters included a 10 cm compacted layer of aggregate material with particle size <150 μm kept at 40% saturation degree with a 10-cm headspace left at the top of the cell. The consumption of the O2 present in the headspace is monitored over a 3-h testing period at 22 °C. The test was able to discriminate the eight sulfide-bearing and control aggregates selected when using a threshold limit of 5% O2 consumed. This draft limit will, however, require to be confirmed through the testing of a larger number of aggregates.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700