Effects of nickel oxide impurities on the microstructure and electrical properties of a nickel-yttria-stabilized zirconia anode
详细信息    查看全文
文摘

Anodes with different NiO powders were imaged using nano-computed tomography.

During co-fired, anode substrate had an influence on anode functional layer.

0.142 wt.% MgO in anode −2 may be the main reason to cause the over-sintering.

The over-sintering can be avoided by lowering the sintering temperature by 50 °C.