Composition and Morphology of Fly Ash Cenospheres Produced from the Combustion of Kuznetsk Coal
详细信息    查看全文
文摘
The chemical and phase composition, morphology, and shell structure of narrow fractions of nonmagnetic and magnetic low-density nonperforated cenospheres separated from fly ash concentrates produced via the pulverized combustion of coal from the Kuznetsk Basin (Russia) have been studied. Narrow fractions of nonmagnetic cenospheres contain 2.6鈥?.5 wt % Fe2O3 and include globules with a uniform smooth or relief surface and shells with different degrees of porosity. For nonmagnetic cenospheres, the aluminum concentration increase leads to an increase in the mullite phase content and a decrease in the average sphere diameter, glass-crystalline shell thickness and porosity, and the crystalline quartz content. The quartz phase comprises two modifications with different lattice parameters. The narrow fractions of magnetic cenospheres contain 3鈥?1 wt % Fe2O3 and include globules with thick porous shells covered by heterogeneous regions of ferrospinel on their outer surface. In magnetic cenospheres, an increase in the iron concentration leads to an increase in the ferrospinel phase content and crystallite size, accompanied by a decrease in the degree of substitution of magnesium and aluminum for iron.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700