摘要
分析某100万t/a乙烯装置中裂解气逆流换热器发生泄漏的原因,阐述裂解气逆流换热器的设计参数和备件设计的改进措施,提出板翅式换热器设计中需注意的几个问题。
        The causes for cracked gas contra-flow heat exchanger of a 100 × 104 t/a ethylene unit is analyzed,the design parameters of the cracked gas contra-flow heat exchanger and improving measures for design of its spare parts are described,and several issues to be noted in design of the plate-fin heat exchanger are pointed.