A study on main limiting factors in sprayed-CZTS solar cells is presented.
Low minority carrier diffusion length values are obtained.
Tunneling enhanced recombination at junction interface explains low Voc values.
A high density of defects at CdS/CZTS junction that favors carrier losses is found.