In Situ X-ray Absorption Spectroscopy Study of the Capacity Fading Mechanism in Hybrid Sn3O2(OH)2/Graphite Battery Anode Nanomaterials
详细信息    查看全文
文摘
In situ X-ray absorption spectroscopy (XAS) of an electrode material under electrochemical control has enabled a detailed examination of the capacity fading mechanism during charge鈥揹ischarge cycling in a hybrid nanomaterial, Sn3O2(OH)2/graphite, that is considered for use as a high-capacity lithium-ion battery anode. By the use of an original one-pot solvothermal synthesis technique, Sn3O2(OH)2 nanoparticles were directly deposited on the surface of nanothin graphite and were charged/discharged in situ for several cycles while XAS spectra at the Sn K-edge were taken. Modeling of the collected extended X-ray absorption fine structure (EXAFS) spectra provides detailed information on the Sn鈥揙, Sn鈥揝n, and Sn鈥揕i coordination numbers and atomic distances for each charged and discharged electrode state. On the basis of electrochemical data and the changes in atomic arrangement deduced from the EXAFS fitting results, including the first unambiguous observation of Sn鈥揕i near neighbors, a capacity fading mechanism is proposed that is different from widely accepted volume expansion for tin metal and tin oxides. Our experimental results suggest that atomic clusters of metallic tin surrounded by highly disordered Li2O shells are formed on first charge. The metallic tin clusters participate in lithiation and delithiation on the following charge/discharge cycles; however, because of continued segregation of tin and Li2O phases, the tin clusters eventually lose electrical contact with the rest of the electrode and become excluded from further participation in electrochemical reactions, resulting in reduced capacity of this anode material.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700