通过共沉淀法制备了钴掺杂的四氧化三铁纳米颗粒,通过对产物的TEM表征,可以看出,产物为粒径为15 nm左右的球形颗粒,结晶很好。同时,对产物进行能谱表征,数据说明钴元素很好地掺杂到了四氧化三铁纳米颗粒中,这对于纳米颗粒的掺杂改性有着重要的意义。
Cobalt doped Fe_3O_4 nanoparticles were prepared by coprecipitation method. Through the TEM characterization of the products,it can be seen that the products are spherical particles with particle size of 15 nm and have good crystallization. At the same time,the products were characterized by energy spectrum. The data indicate that cobalt is well doped into Fe_3O_4 nanoparticles,which is of great significance for the doping modification of nanoparticles.
引文
[1]王建伟.掺杂的Fe3O4纳米晶制备及其性能的研究[D].济南:济南大学,2010.
[2]Suwalka O,Sharma R K,Sebastian V,et al.A study of nanosized Ni substituted Co-Zn ferrite prepared by coprecipitation[J].Journal of Magnetism and Magnetic Materials,2007,313:198-203.
[3]汪汉斌.超小型高分散纳米四氧化三铁粒子的制备及表征[D].武汉:华中科技大学,2004.
[4]朱屯,王福明.国外纳米材料技术进展与应用[M].北京:化学工业出版社,2002.
[5]Zhou Z H,Wang J,Liu X,et al.Synthesis of Fe3O4nanoparticles from emulsions[J].J Mater Chem,2001,11:1704-1709.
[6]王英姿.带能谱分析的扫描电子显微镜在材料分析中的应用[J].制造技术与机床,2007(9):80-82.
[7]张大同.扫描电子显微镜和x摄像微区分析[D].广东:华南理工大学,2009.