摘要
针对核电机组蒸汽发生器管子-管板接头的制造过程,介绍了液压胀接原理。对未胀合缝隙长度过大(欠胀)、胀过、漏胀、重复胀接,以及造成换热管划痕等典型胀接事故进行原因分析,结合工程经验提出预防和纠正措施。
The principle of hydraulic expansion is introduced for the manufacturing process of tube-to-tubesheet joints of nuclear power generator steam generators. The causes of the typical expansion joint accidents such as excessive expansion(under-expansion), over-expansion, leakage expansion, repeated expansion joints and scratches on the heat exchange tubes are combined, and prevention and corrective measures are proposed in combination with engineering experience.
引文
[1]丁训慎.蒸汽发生器传热管的破损及其监督和检查[J].动力工程学报,1997(6):79-85.
[2]压水堆核岛机械设备设计和建造规则:RCC-M-1993[S].
[3]刘振领,戴积林.核电站蒸汽发生器传热管胀接残余应力和残余变形分析研究[C]//全国反应堆结构力学会议.1996.
[4]尹淼晶.AP1000核电蒸发器和非能动换热器管子与管板胀接的数值模拟分析研究[D].上海:华东理工大学,2012.
[5]韩君,杨松,马东华,等.AP1000蒸汽发生器管板群孔高效加工技术方法:103286338A[P].2013-06-18.