ChemInform Abstract: Phase Transition and Thermal Expansion of Ho2W3O12.
详细信息    查看全文
文摘
Polycrystalline Ho2W3O12 is prepared by calcination of stoichiometric amounts of Ho2O3 and WO3 in air (1100 °C, 10 h) with different cooling treatments (850 °C plus furnace cooling or 1100 °C plus quenching in H2O) to probe the relationship between phase formation and preparative conditions.