Ti-6Al-4V welded joint exhibits different fatigue characteristics.

The fatigue crack propagates along α/β boundaries in the BM.

The fatigue crack propagates through α phases and martensite laths in the HAZ.

The fatigue crack propagates along α/β boundaries and martensite laths in the FZ.

Fatigue crack growth rate is fastest in the HAZ, less in the FZ, slowest in the BM.