5–20% of cement was substituted with coal waste (CWP) and its ash (CWA).
Mixes containing up to 5% CWP behaved similar to control mix.
The combination of 7% limestone and CWA enhanced the mix properties.
Relationships obtained as e98cf6ac3">, and e9c8933a38d64ad271aa83ed">, respectively.