Magnetic properties and crystallographic textures of Fe 2.6% Si after 90% cold rolling plus different annealing
详细信息    查看全文
文摘
The effect of rolling and annealing on the crystallographic texture and the magnetic properties of Fe-2.6% Si non-oriented electric steel during 90% cold rolling and different annealing temperature at (600 掳C, 700 掳C, 900 掳C and 1100 掳C) for 60 min and 20 min was analyzed. The 97% hot rolled as received material shows development of alpha and gamma fiber texture affecting on the magnetic properties at rolling and transverse direction. 90% cold rolling with moderate annealing temperature (up to 700 掳C) and 60 min annealing time leads to better textures and improved magnetic properties. Due to coarse grained microstructure after annealing, neutron diffractions is an efficient tool for the analysis of Bulk texture of polycrystalline materials, well known for sufficient grain statistics and bulk texture measurement.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700