Effect of crystal size of ZSM-5 on the aromatic yield and selectivity from catalytic fast pyrolysis of biomass
详细信息    查看全文
文摘
To determine the effect of crystal sizes of ZSM-5 and feedstock species on aromatic yield and selectivity from catalytic fast pyrolysis of biomass, catalytic fast pyrolysis (CFP) of different feedstock species (cellulose, hemicellulose, lignin, pine, corncob and straw) over ZSM-5 with varying crystal size (2 渭m, 200 nm and 50 nm) was conducted in a Pyroprobe pyrolyzer (5200, CDS Analytical). The experimental results show that ZSM-5 with crystal size of 200 nm exhibited the maximum aromatic yield and minimum BTX selectivity. The results could be attributed to its highest micropore surface area, amount of weak acid and maximum Br酶nsted to Lewis acid sites ratio (B/L ratio). Cellulose, hemicellulose and lignin play very different roles in catalytic fast pyrolysis of biomass. Cellulose exhibited the maximum aromatic yield of 38.4% and minimum non-condensable gas yield of 18.4%. Lignin showed the highest coke yield of 68.6% and lowest aromatic yield of 10.2%. And hemicellulose displayed the lowest coke yield of 29.4% and highest yield of non-condensable gas of 39.1%.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700