Pyroplastic deformation of porcelain stoneware tiles: Wet vs. dry processing
详细信息    查看全文
文摘
Several batches of porcelain stoneware were formulated by partial replacement of coarse Na and Na-K feldspars (standard batch) with quartz in two different grain sizes, micronized K-feldspar or a mixture of these components. Everyone was processed (laboratory scale) by wet and dry routes to compare: sintering curve, microstructure, phase composition and viscosity of the liquid phase at high temperature. Pyroplasticity index was determined by 3-point bending test. Results indicate that finer the quartz particles, more they dissolved in liquid phase, increasing viscosity and reducing deformation. Micronized K-feldspar increased the sintering kinetics (causing deformation). However, when K-feldspar was combined with quartz, densification rate was improved without compromising integrity of tile. About dry route, microstructural heterogeneity turned as fundamental to prevent Pyroplastic deformation. As conclusion, pyroplastic deformation occurs by different mechanisms in samples prepared by the two processing routes and bodies prepared via dry route are less likely to undergo pyroplastic deformation.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700