Cerium modified KNBT ceramics were synthesized using the solid-state process.
The d33 and 蟻 of KNBT ceramic were improved by cerium additives.
The tan 未 at high temperature of KNBT ceramic was suppressed by cerium additive.
The d33 and Tc of KNBT-Ce50 ceramic were 28 pC/N and 656 °C, respectively.