The AFA alloy annealed at 1230 °C yields better properties at 700 °C than alloy A1080.
Dislocations can cut L12-ordered precipitates and be pinned by MC precipitates.
Nanoscale precipitates formed during creep testing are crucial to creep/rupture life.