Optimizing electrical poling for tetragonal, lead-free BZT-BCT piezoceramic alloys
详细信息    查看全文
文摘
The piezoelectric properties of tetragonal BZT-BCT materials have been shown to be improved by using the field cooling poling method. It is shown that the piezoelectric coefficient of tetragonal BZT-BCT materials increases with higher poling temperature, and the optimum poling temperature lies near the Curie temperatures for a broad range of compositions. It is also observed from in situ X-ray diffraction measurements with an applied electric field that the magnitude of domain alignment is enhanced with electrical poling at higher electric fields, whereas the remnant ferroelastic domain texture is not affected. Furthermore, these results show a direct correlation between the development of internal bias field, which is induced by the accumulation of defect charge carriers, and the enhanced piezoelectric coefficient. These observations suggest an important role played by the alignment of defect charge carriers in achieving optimum piezoelectric coefficient in lead-free piezoelectric ceramics.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700