Brushite ceramic coatings for dental brace brackets fabricated via aerosol deposition
详细信息    查看全文
文摘
Biocompatible ceramic coatings were fabricated at room temperature by via aerosol deposition (AD), in order to improve the bonding strength between the dental sapphire bracket and the resin. First, the deposition properties of the brushite films coated on the flat sapphire substrate were investigated, confirming their good deposition rate and appropriate adhesive strength. Then, the mesh and check patterns of the coatings were formed on the sapphire brackets in order to obtain a sufficient shear bond strength. The mesh-pattern grown by converging nozzles exhibited a low film thickness (<10 µm) and shear bond strength (<7 MPa) due to the sharp triangular-shaped cross sections. In contrast, the check-pattern showed a high film thickness of ~70 µm at the same deposition time, as well as a high shear bond strength of ~14 MPa, implying that this check-pattern brushite coating formed via the AD process is a promising candidate for application in dental brace brackets.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700