Evolution of hot rolling texture in pure tungsten and lanthanum oxide doped tungsten with various reductions
详细信息    查看全文
文摘

Hot rolled PW and W-1%La2O3 with various strains displayed θ-fiber and γ-fiber textures simultaneously

Dynamic recovery in 72% rolled PW, 43% rolled W-1%La2O3 improved {001}〈110〉 texture

Dynamic recrystallization in 80% rolled PW, 72% rolled W-1%La2O3 improved {001}〈100〉 texture and reduced {111}〈112〉 texture

Occurrence of dynamic recovery and dynamic recrystallization in W-1%La2O3 was sooner than in PW