The effect of the PyC interphase coating on the microwave heating sintered SiC/SiC composites
详细信息    查看全文
文摘

SiC/SiC composites are fabricated by microwave heating at 1100 °C.

SiC/SiC composites are coated with PyC coating of different thickness.

The densification and mechanical properties are discussed.