The oxidation of uranium hydride during its instantaneous or gradual exposure to oxygen
详细信息    查看全文
文摘

Only about 15% of UH3 is oxidised on its gradual exposure to oxygen.

During the gradual exposure of UH3 to oxygen U3O8 rather than UO2 is generated.

For such gradual exposure, predominantly H2 rather than H2O was generated.

For the instantaneous exposure of UH3 to O2 the amount oxidised was variable.

For these experiments, H2 + some H2O was generally produced.

Pyrophoric or non-pyrophoric behaviour was related to “thermal runaway temperature”.