The structure transforms from coarse lamellar to fine lamellar and flake with increasing B.
Electromagnetic stirring by RMF significantly increases the HV, 蟽t and 蟽c.
蟻 increases from 2.0 × 10−8–4.8 × 10−7 惟 m for the increments of T and B studied here.
螖H and CP of the cast sample were calculated as 204.8 J/g and 0.374 J/gK, respectively.