Au(III) reacts with PADA on SDS surface; the Au-PADA complex is fully retained.
The reaction rate is modulated by suitable changes of pH and NaCl concentration.
The reaction at high pH is much faster owing to the high reactivity of the Au(OH)3(H2O) species.
LM-MEUF of the Au(III)-PADA system in SDS provides high extraction yields.