Microstructures and mechanical properties of Al-Li 2198-T8 alloys processed by two different severe plastic deformation methods: A comparative study
详细信息    查看全文
文摘
In this study, the microstructural evolution and mechanical properties of Al-Li 2198-T8 (artificially peak aged) separately processed by two typical severe plastic deformation (SPD) methods (i.e. friction stir processing (FSP) and high-pressure torsion (HPT)) were investigated. The microstructural examination showed that both FSP and HPT were capable of refining the grains for Al-Li 2198-T8, and the HPT processing produced much finer grains. Transmission electron microscopic observation revealed that precipitates of β′ (Al3Zr), θ′ (Al2Cu) and T1 (Al2CuLi) existing in the as-received Al-Li 2198-T8 fully dissolved after HPT, whereas the precipitates of β′ (Al3Zr) were retained in the processed zone after FSP. The hardness and tensile testing demonstrated that the hardness and strength of FSP-processed alloy significantly declined compared to the as-received alloy, while those of HPT-processed alloy substantially increased due to exceptional grain refinement and high dislocation density. The strengthening mechanisms of the alloy before and after the SPD processing were discussed in the present paper.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700