Fluorinated polyimides was deposited on Si wafer with microscale trenches in scCO2.
6FDA and TFDB were used as fluorinated monomers.
Deposition behaviors strongly depended on the feed monomer concentrations at 250 °C.
Slight temperature dependency on deposition behaviors inside trenches was observed.
Phase behaviors inside the reactor were observed during the deposition.