The use of the fracture initiation parameter F1 to predict microcrack nucleation at grain boundaries in Mg-2%Gd alloy
详细信息    查看全文
文摘
listitem" id="list_l0005">

The fracture initiation parameter F1 was used to evaluate the probability of the grain boundary microcrack nucleation

Grain boundaries with larger F1 factor are more likely to cause microcrack nucleation

Extension twinning in the larger grain sized Mg-2%Gd alloy contributed to ductility improvement