We identify the origin of glass forming ability enhanced by atomic size difference.
We examine changes by quantitatively separating the kinetic and thermodynamic contributions.
Larger atomic size differences are found to improve glass forming ability.
Role of atomic size difference is not necessarily to promote kinetic suppression through effective packing.
Atomic size difference could influence GFA by introducing local strains.