The lowest area specific resistance was obtained with Sr = 0.40 and Ta = 0.05.
The activation energies Ea are in the range of 1.3–1.6 eV.
The samples were single phase when Sr = 0, 0.20, 0.40, and 0.6 and Ta = 0.05.
A predictive trend of the electric conductivity is proposed.