Cross-linkable glass-forming twin derivatives of 2-phenylindole were synthesized.
The thermal cross-linking was demonstrated by DSC and ATR-FTIR.
Glass transition temperatures are in the range from 44 to 120 °C.
Hole-drift mobilities exceed 10−4 cm2/Vs.