Coke formation on the surface of Ni/HZSM-5 and Ni-Cu/HZSM-5 catalysts during bio-oil hydrodeoxygenation
详细信息    查看全文
文摘
listitem" id="list_l0005">

Coke formation is the main cause of catalyst deactivation in bio-oil hydrodeoxygenation.

Quantity and species of coke on spent catalysts determine possibility of catalyst regeneration.

Oxygenated compounds and graphitic carbon contained in coke deactivate catalysts.

Cu reduces coke formation for Ni/HZSM-5 catalyst.