Powders will be smaller in the milling process by doping La into the TZM alloy. The average of arc energy and arc time decrease 17.9% and 20.9% due to doping La in TZM alloy. The decrease of defect reflected in mass loss and erosion area reduces 32.5% and 32.6%. The effect of La reduces arc energy by forming reverse current between the contacts.