The main body of the dealloyed S phase remnant has the same crystal structure as S phase.
Copper nanoparticles are present at the intersections of remnant branches.
At the surface of the remnant, a copper layer of ∼2 nm thick is present.
The volume fraction of the dealloyed S phase remnant is 45–60%.