Bismuth iron oxide thin films were grown by atomic layer deposition at 140 °C.
The major phase formed in the films upon annealing at 500 °C was BiFeO3.
BiFeO3 films and films containing excess Bi favored electrical charge polarization.
Slight excess of iron oxide enhanced saturative magnetization behavior.