Pure phase of SrW could be obtained by sintering and subsequent furnace-cooling. Lowering the PO2 suppresses decomposition of SrW during cooling process. Porous structure of sintered body accelerates the decomposition process of SrW. Oxygen deficiency might increase Ms and Ha of SrW.