Chemical and structural changes in polyamide based organic-inorganic hybrid materials upon incorporation of SeS2O62− precursor
详细信息    查看全文
文摘

We investigated deposited and diffused K2SeS2O6 into polyamide 6 (PA 6).

AAS showed Se:S molar ratio = 1:2 within the PA.

Various decomposition products were detected within the polymer.

Measured bandgap shifted towards lower light absorption energies.