Thermodynamics analysis of MoZn system was carried out. A nanopowder MoZn solid solution was obtained by mechanical alloying. After 100 h of MA, MoZn phase was produced with a crystallite size of 36.2 nm. Microhardness properties was obtained for the MA powders.