The ferromagnetic τ-phase has been directly obtained from casting.
The highest Mb>sb> of 117 emu/g was achieved for (Mnb>0.55b>Alb>0.45b>)b>100b>Cb>2b>.
Ball milling increases the coercivity but decreases the magnetic saturation.