Neutral oils like kerosene, diesel, transformer and rapeseed oil were used as collectors or bridging reagents in conventional flotation and oil agglomeration flotation (OAF) process, and a promising OAF process has been developed for the recycling of ultrafine molybdenite resources from the waste tailings. The average size of collected particles (), agglomerates () and their distribution of the froth concentrate were determined by laser particle size analyzer or sieve analysis. Conventional flotation froth cannot catch the ultrafine particles, so it is an ineffective process to recover molybdenum metal in the waste tailings, while OAF has some advantages to recover fine minerals. And the best result was obtained from transformer oil due to its appropriate length of carbon chain, kinematic viscosity and cyclical structure. The oil amount plays a very important role on average size of the particles, with the increase of transformer oil from 2.0 to 13.8 kg/t, increases from 0.15 to 0.68 mm and decreases from 9.06 to 2.05 ¦Ìm. This finding suggests the bigger the , the smaller the , and the higher the recovery of molybdenite.

The appropriate conditions for recovering ultrafine molybdenite were determined as follows: dosage of frother: 0.5 kg/t, natural pH: 6.2, stirring time: 3 min, and stirring intensity:400-600 r/min. Lastly, the closed cycle test and industrial application in the producing scale of 500 t/d were carried out, and result shows 95 % molybdenum was recovered with a satisfied grade of 22.62 % .

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700