Laser metal deposition of TiC/Inconel 718 composites with tailored interfacial microstructures
详细信息    查看全文
文摘
Laser metal deposition (LMD) was applied to deposit Inconel 718 metal matrix composites reinforced with TiC particles. The influence of laser energy input per unit length on constitution phases, microstructures, hardness, and wear performance of LMD-processed TiC/Inconel 718 composites was studied. It revealed that the LMD-processed composites consisted of ¦Ã Ni-Cr solid solution matrix, the intermetallic precipitation phase ¦Ã¡ä, and the TiC reinforcing phase. For the laser energy input per unit length of 80-120 kJ/m, a coherent interfacial layer with the thickness of 0.8-1.4 ¦Ìm was formed between TiC reinforcing particles and the matrix, which was identified as (Ti,M)C (M=Nb and Mo) layer. Its formation was due to the reaction of the strong carbide-forming elements Nb and Mo of the matrix with the dissolved Ti and C on the surface of TiC particles. The microstructures of the TiC reinforcing phase experienced a successive change as laser energy input per unit length increased: Relatively coarsened poly-angular particles (80 kJ/m) - surface melted, smoothened TiC particles (¡Ý100 kJ/m) - fully melted/precipitated, significantly refined TiC dendrites/particles (160 kJ/m). Using the laser energy input per unit length ¡Ý100 kJ/m produced the fully dense composites having the uniformly dispersed TiC reinforcing particles. Either the formation of reinforcement/matrix interfacial layer or the refinement in TiC dendrites/particles microstructures enhanced the microhardness and wear performance of TiC/Inconel 718 composites.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700