Three methods for moisturizing anode are proposed when neat methanol is used.
A quasi-superhydrophobic SPMP is applied as a water management layer.
Enhancing WBD by use of a cathode SPMP is the most effective way.
WBD flux is determined in a fully passive way.
Performance degeneration in the early discharging stage can be eliminated.