Preparation of ultra-fine grain W-Y2O3 alloy by an improved wet chemical method and two-step spark plasma sintering
详细信息    查看全文
文摘
Average tungsten grain size of 10.7 nm was obtained for the powder precursor. Nano Y2O3 particles were uniformly dispersed within tungsten matrix. The Vickers microhardness of sintered W- Y2O3 alloy is up to 1078.31 Hv.