The aim of the present study was to investigate the effects of low-temperature aging on the micro-mechanical and micro-structural properties of zirconia-porcelain interface. In total, thirty-three Y-TZP zirconia blocks were fabricated by using CAD/CAM technology, veneered with porcelains. Specimens were submitted to low-temperature aging in an autoclave at 134 °C, additional 0.2 MPa pressure for 0 h, 5 h, or 10 h. Flexural strength was obtained by using three-point bending test. Micro-mechanical properties (nano-hardness (H) and reduced modulus (Er)) were investigated by nanoindentation tests. Scanning electron microscopy and X-ray diffraction analyses were performed to identify the micro-structure and fracture behavior. The flexure strength, modulus and hardness of zirconia increased after 5 h aging and decreased after 10 h aging. No significant alterations of the reduced modulus or hardness of porcelain were detected in the whole aging duration. Width of the zirconia-porcelain interface was extended towards the bulk of zirconia. The detachment and cracks could be observed in zirconia, and the crystal alignment was disorganized in porcelain after 5 h aging and 10 h aging. Mechanical properties of the veneering porcelain are not affected by low-temperature aging. However, the expansion and the alterations of micro-mechanical and micro-structural properties of zirconia-porcelain interface were detected.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700