Substrates with various characteristics of surface microstructure were prepared.
The development rules of surface microstructure were analyzed.
The main factors of surface microstructure on loading effect were evaluated.
Photocatalytic testing was conducted to prove the optimal surface microstructure.
Specimen of 14-days curing ages showed the best degradation efficiency.