Examples of luminescent phosphors yielding intense TA-OSL have been presented.
Using TA-OSL it is possible to measure doses of few tens of kGy.
Aluminum oxide and quartz exhibit very interesting TA-OSL features.
Further TA-OSL studies are required, especially in feldspars and polymineral samples.