Long-term durability of HT-PEM fuel cells based on thermally cross-linked polybenzimidazole
详细信息    查看全文
文摘
High temperature PEMFC durability studied under steady state conditions for over 13,000 h. Well defined beginning-of-life and end-of-test with minimal operational disturbance. Lowest degradation rate of 0.5 μV h−1 within first 9200 h reported for cross-linked membranes. Average voltage decay rate of about 1.4 μV h−1 with 13,000 h versus 4.6 μV h −1 for reference. EIS and post mortem analysis showed improved acid retention of the cross-linked membrane.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700