Experimental research on swelling and glass transition behavior of poly(methyl methacrylate) in supercritical carbon dioxide
详细信息    查看全文
文摘

The volume change ratio of PMMA at 12 MPa has the most significant increment, instead of that at 20 MPa.

Tg of PMMA decreased from 380.5 to 311.4 K withCO2 pressure 0.1–12 MPa, and increased from 311.4 to 323.1 K with 12–22 MPa.

When CO2 pressure is beyond 12 MPa, hydrostatic pressure has a more significant effect on swelling ratio than swelling.

The g" data-mathURL="/science?_ob=MathURL&_method=retrieve&_eid=1-s2.0-S0896844615302151&_mathId=si1.gif&_user=111111111&_pii=S0896844615302151&_rdoc=1&_issn=08968446&md5=43049a56100f51066de64d2608745823" title="Click to view the MathML source">Tsat−pCO2 curve has similar change with the g" data-mathURL="/science?_ob=MathURL&_method=retrieve&_eid=1-s2.0-S0896844615302151&_mathId=si2.gif&_user=111111111&_pii=S0896844615302151&_rdoc=1&_issn=08968446&md5=2751382d08fe9d5c7ff335264c66ecbe" title="Click to view the MathML source">Tg−pCO2 curve.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700