Microstructure and thermoelectric properties of WSib>2b>-added CrSib>2b> composite
详细信息    查看全文
文摘
bel">•

CrSib>2b>-based composites were fabricated by the WSib>2b> addition.

bel">•

Grain size of CrSib>2b> phase was effectively reduced by the WSib>2b> addition.

bel">•

The composite effects induced by the WSib>2b> addition effectively reduced κ of CrSib>2b>.

bel">•

The WSib>2b> addition had little effect on the thermoelectric power factor.

bel">•

ZT value was enhanced and reached 0.3 around 700 K.