SrMo0.94Fe0.06O3−δ is compatible with Gd0.2Ce0.8O1.9 in both air and H2 atmosphere.
SrMo0.94Fe0.06O3−δ can be easily obtained by reducing SrMo0.94Fe0.06O4−δ at 850 °C.
The ionic conductivity can be improved by adding GDC into SrMo0.94Fe0.06O3−δ.
The lowest RP of composite anode can be obtained by suitable GDC adding.
SMF7-GDC3 has favorable electrochemical catalytic activity of hydrogen oxidation.