Microstructure and oxidation behavior of Al + Cr co-deposited coatings on nickel-based superalloys
详细信息    查看全文
文摘
Co-deposition coatings were prepared by a one-step pack cementation process. The single chromized coatings had good oxidation resistance at 950 °C. Higher Cr contents in the coatings stimulate the formation of Al2O3.