High temperature oxidation behavior and wear resistance of Ti0.53Al0.47N coating by cathodic arc evaporation
详细信息    查看全文
文摘
High-temperature wear tests of the Ti0.53Al0.47N coatings were carried out. The maximum test temperature was elevated to 850 °C during the wear test. XPS analysis and AES depth profiling of the oxide scales formed at RT–850 °C. Relationship between wear mechanism and working temperature was discussed.